Sample Set for Microcement

Sample Set for Microcement

Microcement in medium grain size and up to 10 custom colors of your choice. Ideal for testing!

Delivery time: 1-3 business days | Free shipping on orders over $50

You’re interested in our microcement but want to test its quality and application beforehand? – Then our “Sample Set for Microcement” is perfect for you!
This set includes 15.4lbs of microcement powder in medium grain size (A-Component) and 4.4lbs of liquid acrylic resin (B-Component). This is sufficient to apply 2 layers on an area of 37.6sqft. In addition, you can add up to 10 colors to your set to try out different colors. This way, you’re guaranteed to find the right shade for your project.

Product Properties
Application
Product Description Microcement, nano concrete, design levelling compound
Area of Application Area of Application almost any walls and floors, furniture, facades, stairs, industrial halls, cellars etc.
Field of Application Indoor & Outdoor use and damp rooms
Method of application Trowel
Self-levelling minimal; must be spread and smoothed out with a trowel
Consumption Quantity Floor Layer 1 (large-grained): 0.32lb/sqft, Layer 2 (medium-grained): 0.24lb/sqft
Consumption Quantity Wall Layer 1 (medium-grained): 0.24lb/sqft, Layer 2 (medium-grained): 0.24lb/sqft
Odour development during application Low (according to amine)
Spray and Drip Behaviour Depending on processing consistency, dripping possible on wall surfaces
Application Temperature Substrate and ambient temperature must be min. 50°F and max. 85°F
Optimum Processing Temperature 70°F
Mixing ratio by weight Powder (A): Liquid (B) Medium: 100:20, Large: 100:25
Pot Life at 70°F 120 minutes for 22lbs
Recommended layer thickness Medium and large 1/16"
Recommended number of layers min. 2 layers
Waiting time between layers max. 24 hours
Waiting time before painting over with another product (i.e. PU Sealant) after 48 hours
Primer on absorbent, even substrates Deep Primer recommended
Primer on non-absorbent, even substrates 2K Bonding Primer
Leveling and priming of floors 2K Leveling compound
Leveling and priming of walls Putty Primer
Max. humidity level during application 60%
Technical Properties
Material Base Cement
Component A Powder for Microcement and Quartz
Component B Acrylic Resin in Water Dispersion
Gloss Level Satin; Matte finish possible with PU sealer
Consistency High viscosity, viscosity can be adjusted depending on the amount of LIQUID (B) added.
Coverage Highly Opaque
Surface Finish Highly durable, abrasion-resistant, hard-wearing, scrub-resistant
Scratch Resistance/Abrasion Resistance Reinforced by the application of PU and recommended for heavily used surfaces and wet areas
Compressive Strength after 7 days ≥ 12.0 MPa (EN 13892-2)
Compressive Strength after 28 days ≥ 20 MPa (EN 13892-2)
Flexural Strength after 7 days 4.0 MPa (EN 13892-2)
Flexural Strength after 28 days 7.0 MPa (EN 13892-2)
Fire resistance class Efl EN 13501-1
Shore Hardness ≥80
Elasticity1 Not elastic; glass fibre mesh must be incorporated on substrate susceptible to vibrate
Open to diffusion, breathable Yes (unless extra PU sealant are applied)
Application in Wet Areas Not recommended without PU sealant in wet areas
Color Fastness High
Color Intensity High
Grain Finish Medium
UV-resistant UV-Stable
Solvent-Free Yes
Plasticiser-Free Yes
VOC-Free Yes
Susceptible to abrasion marks and gloss spots (so-called writing effect) Low (Touch-Protect-System)
Environmentally Friendly Yes
Pigment Content 2-10% depending on desired color intensity, recommended 2%
Density (oz/inch³) 182 - 1295oz/inch³
Maximum Grain Size Large (450µm), Medium (330µm)
Dilutable Medium: max. 100:23, large: max. 100:28
Tool Cleaning Tool Cleaning Immediately after use with acetone/thinner
Chemical Resistance Acids, alkalis and chlorine should be avoided
Surface Cleaning Light surfactants (do not use acidic or chlorinated cleaners or alkaline solutions)
Storage Temperature Airtight, cool, dry, and frost-free
Max. Storage Temperature 75°F
Min. Storage Temperature 50°F
Minimum Shelf Life Unopened 12 months, Open 6 months
  1. If the substrate presents expansion joints, these must be taken into account when applying microcement. The expansion joint must either be reinforced with fibre glass mesh or a joint must be included into the microcement. Rooms larger than 535sqft should always include expansion joints. Ignoring existing expansion joints or not including them when needed can lead to the microcement cracking.
SKU: set-mz-10-farben Categories: ,

Microcement Seemless Design

EPODEX Microcement is a special easy-to-apply leveling compound. It can be applied onto floors, walls, stairs, table, and more! Acchieve a unique, comtemporary interior decor in no time. From exposed concrete wth natural cavities to multi-colored designs with 3D effect - Everything is possible!

Universally Applicable

Our microcement is suitable for indoor and outdoor use and can be applied to almost all substrates such as parquet, tiles, natural stone, plasterboard, metal, ceramic, marble, OSB and more. The material is highly resilient and UV-resistant. At the same time, it remains flexible and breathable.

Completely Waterproof

EPODEX microcement in combination with our polyurethane resin (PU) sealant is waterproof and weather resistant. It is therefore ideal for showers and outdoor areas. The sealing layer is finally rolled onto the hardened microcement.
pu polyurethane resin matte
Add Accessories

Get the service you deserve!

Guaranteed hassle-free shopping experience. Simply select the color and the square footage you want to cover. We automatically calculate the required amount of microcement and dye for you.
No surprises. You always get the color you see online. We present all our colors in 4K videos and high-resolution pictures so you can see exactly what you are getting.
Professional easy to follow step-by-step tutorials.
Same Day Shipping
Delivery across USA
Friendly 24h-Support


Instructions for Use

Primer

  1. The substrate must be stable, dry, and free of dirt, separating agents, and coarse unevenness.
  2. Sand off any unevenness.
  3. If required use our Putty Primer on your walls and 2K Leveling Compound on your floor to level and prime, for example on tiles.
  4. If your area to be coated is already leveled and smooth, use either our 2K Bonding Primer (for-non absorbent surfaces) or DEEP PRIMER (for absorbent surfaces) to prime your furniture.

Main Coating

  1. Mix microcement A components with the Liquid B component in the mixing ratio specified on the label.
  2. Add 2% WB pigment to color the material (i.e. 2×3.5oz WB Pigment to 1 bag microcement powder and its liquid B-component).
  3. Spread the material thinly with a trowel and allow to dry.
  4. Sand off any unevenness in the surface greater than 1/8″ and vacuum up any sanding dust.
  5. Apply a second coat in the same way within 24 hours.
  6. Application of microcement on walls: Layer 1 (medium grain size): 0.24lb/sqft, Layer 2 (medium grain size): 0.24lb/sqft
    Application of microcement on a floor: Layer 1 (large grain size): 0.32lb/sqft, layer 2 (medium grain size): 0.24lb/sqft

Pro Tip: Up to 10% WB Pigment can be added for more intense colors. If you exceed 24 hours between the microcement layers, sand the first layer and remove the dust. This roughens the surface for better bonding and ensures the next layer won’t break off.
For stubborn fine particles, use a light brush of liquid B. Brush or roll on a small amount to avoid flooding the surface.


Sealant

Note: For damp rooms, surfaces in direct contact with water and heavily used surfaces (high mechanical stress, cleaning with aggressive cleaning agents, etc.), we recommend sealing the surface with EPODEX matte polyurethane resin (PU resin).

  1. Wait at least 48 hours after the last microcement layer before proceeding with the PU sealant.
  2. The temperature of the room, the substrate, and the PU must be at least 60°F.
  3. Make sure that the substrate is clean, dry, and free of any substance that may prevent the PU’s adhesion.
  4. Coat the surface with the PU resin.
  5. To do this, mix the PU resin (A) with PU hardener (B) in a 10:1 ratio by weight (e.g.: 10oz A + 1oz B).
  6. Transfer the mixture to a paint tray and mix again. This way you make sure that resin (A) and hardener (B) mix completely.
  7. We recommend mixing smaller quantities (max. 35oz at once), as the material, is very reactive and sets quickly (pot life: 60 min. for 35oz).
  8. Apply the material very thinly with a foam roller in a criss-cross pattern. To achieve an even finish, use our scraper grid to scrape off excess material before application. We recommend a layer thickness of max. 150µm. If the coat is too thick, the PU won’t cure properly.
  9. The material can be walked on after approx. 20-24 hours and is completely chemically cured after approx. 7 days.

Pro Tip: To ensure that your PU is applied everywhere, apply the quantity received in 2 coats. By applying 2 coats in a criss-cross motion, the chance of an unsealed gap is greatly reduced.


Customer Service: If you have further questions, please contact us by phone, e-mail or use our WhatsApp support.

Note: Please note that due to different lighting conditions and monitors, the colors may not be uniformly displayed.

5 11 reviews
1
0%
2
0%
3
0%
4
0%
5
100%